Adhesion promotion of fluorocarbon films
Filed: January 4th, 1995 [Granted]
Patent Number: 5549935
The C2F4 feed is continued at the above conditions for about 20 minutes to provide a polymerized fluorocarbon film of about 0.6 microns thick.
Method for depositing fluorocarbon films on polymer surfaces
Filed: April 27th, 2007 [Granted]
Patent Number: 7879418
1 METHOD FOR DEPOSITING FLUOROCARBON FILMS ON POLYMER SURFACES STATEMENT AS TO RIGHTS TO INVENTIONS 5 MADE UNDER FEDERALLY SPONSORED RESEARCH OR DEVELOPMENT ...
Promotion of the adhesion of fluorocarbon films
Filed: November 15th, 1995 [Granted]
Patent Number: 5788870
For instance, the plasma deposition of the range of about 10 to about 180 mXorr ^ more typicauy & polymeric fluorocarbon film can be earned out in a chamber ...
Method for fluorocarbon film depositing
Filed: June 24th, 2002 [Pending]
Patent Application Number: 10178910
As an example, a fluorocarbon film may be produced by ionizing a fluorocarbon gas in a plasma reactor and then depositing the ionized gas onto an integrated ...
Thin amorphous fluorocarbon films
Filed: January 22nd, 1999 [Granted]
Patent Number: 6528865
4, 2003 (54) THIN AMORPHOUS FLUOROCARBON FILMS (75) Inventor: Indrajit Banerjee, San Jose, CA (US) (73) Assignee: Intel Corporation, Santa Clara, ...
Lamination of fluorocarbon films
Filed: October 28th, 1983 [Granted]
Patent Number: 4549921
... OF FLUOROCARBON FILMS [75] Inventor: William R. Wolfe, Jr., Wilmington, Del. [73] Assignee: EI Du Pont de Nemours and Company, Wilmington, Del.
FLUOROCARBON FILM AND PROCESS FOR ITS PRODUCTION
Filed: May 2nd, 2007 [Pending]
Patent Application Number: 11743260
Here, the wiping efficiency being good means that the water repellency of the fluorocarbon film is good, such efficiency being maintained even after the ...
Fluorocarbon film and method for forming same
Filed: November 9th, 2004 [Granted]
Patent Number: 7648922
11 400° C. for 1 hour, a fluorocarbon film having a specific inductive capacity of 1.5 was obtained. Since decrease in the film thickness can be suppressed ...